Ceramic Inclusion Stains

Sino's inclusion stains solve the problem that cadmium red can't resist high temperature.

They are very stable in the glaze which contains lead, calcium, or boron. If the content of the alkali metal in the giaze is too high, it will damage the included layer of the stains, and also degrade the color. So the grinding of the stain can't last long time.

The temperature range covers: 800°C-1280°C

Code No. Name Composition Max Firing Temp Firing condition Color
SIS300B Pale yellow Cd-Si-Zr-S 1280 Oxide  
SIS300 Yellow Cd-Si-Zr-S 1280 Oxide  
SIS300A Dark yellow Cd-Si-Zr-S 1280 Oxide  
SIS301C Orange yellow Cd-Si-Zr-Se-S 1280 Oxide  
SIS301 Orange yellow Cd-Si-Zr-Se-S 1280 Oxide  
SIS301A Orange yellow Cd-Si-Zr-Se-S 1280 Oxide  
SIS301B Orange red Cd-Si-Zr-Se-S 1280 Oxide  
SIS306 Red Cd-Si-Zr-Se-S 1280 Oxide  
SIS306A Red Cd-Si-Zr-Se-S 1280 Oxide  
SIS306B Red Cd-Si-Zr-Se-S 1280 Oxide  
SIS306C Dark Red Cd-Si-Zr-Se-S 1280 Oxide  
SIS309 Dark Red Cd-Si-Zr-Se-S 1280 Oxide